Slax

SiO2

Al2O3

Fe2O3

MgO

L.O.I

CaO

MnO

TiO2

Oxide

55.35%

14.07%

2.78%

3.86

15.2%

1.09%

0.016%

0.54%

%

 

 

It is simple to use convenient, usually in casting process for water bubble filled the product and in the liquid metal surface. Also can be in application of electrothermal furnace, should be in melting quickly end, liquid metal before in the oven and from the liquid metal surface, the surface to pick out the slagging can.